Blog

Koj ntsuas Skid Resistance ntawm Txoj Kev Li Cas?

Aug 20, 2026 Tso lus

Core Takeaways: Yuav ua li cas Pavement Skid Resistance yog ntsuas tiag tiag

 

Skid resistance of road surfaces piav qhia txog kev sib txhuam kev ua tau zoo ntawm lub log tsheb lossis cov qauv roj hmab slider thiab qhov chaw pavement. Rau cov kws tshaj lij, cov lus nug tseem ceeb tsis yog tsuas yog seb txoj kev taug kev yog "nruj" lossis "ntu", tab sis seb nws qhov chaw puas tuaj yeem muab kev sib txhuam txaus raws li cov xwm txheej tau teev tseg los ntawm txoj kev xeem siv.

 

Pendulum Skid Tester muab ib txoj hauv kev los ntsuas qhov kev sib txhuam ntawm thaj chaw hauv cheeb tsam. Hloov chaw ntawm lub tsheb, cov cuab yeej tseem nyob ruaj khov ntawm qhov chaw sim thaum lub roj hmab slider mounted ntawm qhov kawg ntawm lub pendulum caj npab txav hla qhov chaw kuaj. Qhov tshwm sim lub zog poob muab cov qauv qhia ntawm qhov chaw sib txhuam cov yam ntxwv. ASTM E303 txheeb xyuas British Pendulum Tester raws li qhov cuam tshuam pendulum dynamic-type tester haum rau ob qho tib si kuaj thiab kuaj teb.

 

The Pendulum Skid Tester is a stationary portable instrument designed for localized friction testing on pavement and other surfaces

Pendulum Skid Tester yog ib qho khoom siv ruaj khov, nqa tau yooj yim tsim los rau kev ntsuas kev sib txhuam hauv zos ntawm txoj kev pavement thiab lwm qhov chaw.

 

 

Skid Resistance of Road Surfaces yog dab tsi?

Vim li cas Surface Friction Matters rau Txoj Kev Nyab Xeeb?

Skid resistance yog qhov tseem ceeb cuam tshuam nrog kev sib cuam tshuam ntawm lub log tsheb thiab cov pavement. Thaum lub tsheb nres, nrawm, lossis hloov cov kev taw qhia, lub zog yuav tsum raug xa mus los ntawm thaj chaw me me ntawm lub log tsheb thiab txoj kev. Yog tias muaj kev sib txhuam tsis txaus rau qhov kev thov, lub log tsheb yuav tshwm sim.

 

Cov dej ntub dej ua rau qhov teeb meem no tseem ceeb dua. Cov dej tuaj yeem txo qhov kev sib cuag ncaj qha ntawm lub log tsheb thiab txoj kev taug kev, tshwj xeeb tshaj yog thaum lub npoo tsis txaus los yog thaum cov pavement tau polished los ntawm kev khiav tsheb. Yog li ntawd, cov neeg ua haujlwm pavement niaj hnub tshawb xyuas cov yam ntxwv ntawm kev sib txhuam thaum ntsuas kev nyab xeeb thiab kev ua haujlwm saum npoo av.

 

Txawm li cas los xij, kev tiv thaiv skid yuav tsum tsis txhob tsis meej pem nrog pavement roughness. Roughness feem ntau piav qhia txog qhov ntev ntawm qhov tsis sib xws thiab cuam tshuam rau kev caij tsheb zoo, thaum kev sib tw tsis zoo piav qhia txog kev sib txhuam ntawm qhov chaw pavement. Ib txoj kev tuaj yeem muab kev caij tsheb du thaum tseem muaj kev sib txhuam tsis txaus.

Microtexture tseem ceeb tshwj xeeb rau kev ntsuas Pendulum

Kev ntxhib los mos ntawm qhov chaw muaj nyob ntawm qhov sib txawv. Microtexture hais txog qhov me me - nplai roughness ntawm aggregate hais, thaum macrotexture sawv cev loj dua nta uas ua rau cov dej ntws thiab cov log tsheb sib cuag.

 

Txoj kev British Pendulum tshwj xeeb yog txuam nrog kev ntsuas cov khoom sib txhuam ntawm qhov chaw microtexture. ASTM E303 piav qhia meej txog qhov kev ntsuam xyuas raws li kev ntsuas ntawm cov khoom sib txhuam, microtexture, ntawm qhov chaw hauv chav kuaj lossis thaj chaw.

 

Qhov kev sib txawv no tseem ceeb thaum txhais cov txiaj ntsig. Kev ntsuas pendulum yuav tsum tsis txhob raug kho raws li cov lus piav qhia tag nrho ntawm txhua qhov ntawm txoj kab kev ntxhib los mos. Rau kev tshawb nrhiav txog kev taug kev, cov kws tsim qauv tuaj yeem sib txuas cov kev ntsuas kev sib txhuam nrog cov kev ntsuas macrotexture, kev sim sib sau ua ke, kev tshuaj xyuas qhov muag, thiab lwm yam pavement - cov ntaub ntawv ua haujlwm.

 

Lub Pendulum Skid Tester ntsuas qhov kev sib txhuam li cas?

Txoj Cai Ua Haujlwm ntawm Pendulum Skid Tester

Lub hauv paus ntsiab lus ntawm kev khiav hauj lwm yog qhov yooj yim tab sis mechanically meej. Ib tug qauv roj hmab slider yog mounted nyob rau hauv kawg ntawm ib tug pendulum caj npab. Lub pendulum raug tsa mus rau qhov chaw pib thiab tso tawm kom lub slider hla mus rau qhov chaw kuaj.

 

Raws li cov roj hmab slider txav mus rau saum npoo, kev sib txhuam ua rau lub zog poob ntawm lub pendulum. Qhov ua rau txo qis hauv lub pendulum lub zog yog cuam tshuam nrog kev sib txhuam cov yam ntxwv ntawm qhov ntsuas qhov chaw.

 

Qhov no yog qhov txawv ntawm lub tsheb -mounted kev sib txhuam tester. Pendulum Skid Tester tsis tas yuav taug kev raws txoj kev thaum ntsuas kev sib txhuam. Hloov chaw, nws ntsuas qhov chaw xaiv ntawm qhov ntsuas tau muab tso rau.

 

BS EN 13036-4 piav qhia txog kev ntsuas pendulum raws li ib txoj hauv kev uas cov cuab yeej tseem nyob ruaj khov ntawm qhov chaw sim thiab siv lub slider mounted ntawm qhov kawg ntawm caj npab pendulum.

Yog vim li cas qhov chaw nres tsheb ntsuam xyuas teeb meem

Kev teeb tsa nyob ruaj ruaj ua rau Pendulum Skid Tester tshwj xeeb tshaj yog muaj txiaj ntsig zoo thaum cov kws ua haujlwm xav tau los tshawb xyuas qhov chaw tshwj xeeb es tsis yog kev tshawb fawb ntau mais txuas ntxiv.

 

Piv txwv li, tus kws ua haujlwm yuav txheeb xyuas qhov chaw uas muaj feem cuam tshuam ze ntawm qhov kev sib tshuam, kev hla kev taug kev, txoj kev choj, txoj kev, lossis thaj chaw kho qhov chaw. Cov cuab yeej tuaj yeem muab tso ncaj qha rau ntawm qhov chaw xaiv thiab siv kom tau txais kev ntsuas kev sib txhuam hauv zos.

 

Tib lub hauv paus ntsiab lus tseem ceeb hauv chav kuaj, qhov twg asphalt specimens, paving cov ntaub ntawv, flooring nto, los yog lwm yam kev ntsuam xyuas qhov chaw yuav raug soj ntsuam nyob rau hauv kev tswj tej yam kev mob.

 

The tester remains stationary while the pendulum slider travels across a defined area of the surface allowing engineers to investigate specific pavement locations

Lub tester tseem nyob ruaj ruaj thaum lub pendulum slider mus hla ib cheeb tsam ntawm qhov chaw, cia cov engineers tshawb xyuas qhov chaw pavement.

 

Dab tsi yog Pendulum Skid Tester ntsuas qhov tseeb?

Nkag siab txog BPN thiab Pendulum Test Results

Ib qho ntawm cov ntsiab lus tseem ceeb tshaj plaws thaum siv British Pendulum-type tester yog nkag siab tias tus nqi tshaj tawm yog dab tsi. ASTM E303 txheeb xyuas BPN, lossis British Pendulum Number, raws li tus nqi tau txais rau qhov chaw tiaj tus siv British Pendulum Tester.

 

Cov txiaj ntsig yuav tsum raug txhais raws li kev ntsuas uas tsim los ntawm cov cuab yeej thiab cov txheej txheem. Nws yuav tsum tsis txhob cia li hloov mus rau hauv universal kev sib txhuam coefficient los yog kho raws li tus lej sib pauv nrog cov txiaj ntsig tau los ntawm lwm qhov kev sib txhuam- txoj kev sim.

ASTM tshwj xeeb ceeb toom tias cov txiaj ntsig tau txais los ntawm British Pendulum txoj kev tsis tas yuav pom zoo lossis cuam tshuam ncaj qha nrog rau lwm txoj hauv kev txiav txim siab kev sib txhuam lossis kev sib tw.

 

Qhov no yog ib qho tseem ceeb rau kev txiav txim siab thaum sib piv cov ntawv xeem los ntawm ntau lub chaw soj nstuam. Ua ntej sib piv ob qhov tseem ceeb, cov kws tsim khoom yuav tsum xyuas kom meej tias tib txoj kev sim, kev teeb tsa slider, qhov chaw nyob, thiab cov txheej txheem qhia tau siv.

Yog vim li cas ib tug xov tooj Friction tsis yog tag nrho Pavement Story

Cov txiaj ntsig qis qis qhia tau tias muaj kev sib txhuam- tus yam ntxwv ntsig txog ntawm qhov chaw sim, tab sis nws tsis yog nws tus kheej txheeb xyuas qhov laj thawj. Kev sib txhuam polishing, kev sib kis, hnav khaub ncaws saum npoo, ntau dhau ntawm qhov chaw, kev ntxhib los mos tsis zoo, lossis lwm yam pavement tej zaum yuav cuam tshuam qhov tshwm sim.

 

Yog li ntawd, thaum kuaj pom tus nqi qis, cov lus teb tsim nyog yog kev tshawb xyuas es tsis yog tam sim ntawd xav tias tag nrho cov pavement seem tau ua tsis tiav.

 

Koj Ua Li Cas Pavement Skid Resistance Test?

Npaj Kev Xeem Nto

Kev ntsuam xyuas ntseeg tau pib nrog kev npaj kom raug ntawm qhov chaw xeem. Qhov saum npoo yuav tsum yog tus neeg sawv cev ntawm tus mob uas raug tshawb xyuas, thiab cov khib nyiab xoob, cov kab mob sib kis ntau dhau, lossis lwm yam khoom siv txawv txav yuav tsum tau sau tseg thiab kho raws li cov txheej txheem xeem.

 

Qhov kev kuaj xyuas tseeb, qhov xwm txheej slider, dej txias, thiab cov txheej txheem ntsuas yuav tsum ua raws li tus qauv teev tseg rau qhov project.

 

Rau kev tshawb nrhiav hauv cheeb tsam, engineers yuav tsum tau sau qhov chaw thiab cov xwm txheej ib puag ncig kom cov kev ntsuas tom ntej tuaj yeem muab piv rau qhov muaj txiaj ntsig.

Muab tso rau thiab teeb tsa Pendulum Tester

Qhov ntsuas tau muab tso rau ntawm qhov chaw kuaj kom zoo thiab kho kom lub pendulum mechanism ua haujlwm kom raug. Tus tester yuav tsum ruaj khov vim tias kev txav ntawm lub hauv paus thaum lub pendulum viav vias tuaj yeem qhia qhov yuam kev.

 

Lub pendulum caj npab thiab roj hmab slider ces yuav tsum tau npaj raws li cov txheej txheem siv. Slider mob yog qhov tseem ceeb tshwj xeeb vim tias qhov kev sib txhuam teb nyob ntawm kev sib cuam tshuam ntawm cov qauv siv roj hmab thiab qhov chaw kuaj.

 

Cov cuab yeej muab los ntawm Tianpeng yog tsim nyob ib ncig ntawm lub pendulum nyob ruaj ruaj no - kev sim txoj cai, nrog rau cov ntaub ntawv khoom siv qhia txog kev siv rau ob qho tib si kuaj thiab ntawm - qhov chaw kuaj qhov chaw.

Kev ntsuas rov ua dua

Kev xeem kws tshaj lij yuav tsum tsis txhob cia siab rau ntawm ib lub viav vias uas tsis tswj tau. Cov txheej txheem xeem uas siv tau los tsim kom muaj qhov ntsuas qhov ntsuas li cas, ntsuas ntsuas li cas, thiab ntsuas qhov rov ua dua li cas.

 

Kev ntsuas rov qab muaj txiaj ntsig zoo vim tias lawv tso cai rau tus neeg teb xov tooj txheeb xyuas qhov kev nyeem ntawv txawv txav thiab ntsuas qhov sib xws. Yog tias kev ntsuas sib txawv heev, tus neeg teb xov tooj yuav tsum tshawb xyuas qhov xwm txheej ntawm qhov chaw, qhov chaw slider, kev teeb tsa, lossis cov txheej txheem kuaj ua ntej lees txais qhov kawg tshwm sim.

 

Correct positioning and controlled operation are essential because the Pendulum Skid Tester evaluates a relatively small localized area of the pavement surface

Kev ua haujlwm kom raug thiab tswj tau yog qhov tseem ceeb vim tias Pendulum Skid Tester ntsuas qhov me me, thaj chaw ntawm thaj chaw pavement.

 

 

Cov qauv twg yog siv rau Pendulum Skid Resistance Test?

ASTM E303 thiab British Pendulum Tester

ASTM E303 yog ib qho ntawm cov qauv pom zoo tshaj plaws nrog rau British Pendulum Tester. Daim ntawv teev npe ASTM tam sim no txheeb xyuas ASTM E303-22, Kev Ntsuas Tus Txheej Txheem rau Kev Ntsuas Cov Khoom Sib Cuam Ntog Siv Cov Khoom Siv Hluav Taws Xob British Pendulum Tester. Lub peev xwm npog qhov ntsuas ntawm qhov sib txhuam ntawm qhov chaw siv lub British pendulum skid resistance tester thiab suav nrog cov txheej txheem calibration.

 

Tus qauv kuj tseem hais tias cov cuab yeej tsim nyog rau kev sim thiab kev sim teb rau ntawm qhov chaw tiaj tus. Qhov no ua rau txoj kev muaj txiaj ntsig tshwj xeeb thaum lub hom phiaj yog txhawm rau tshawb xyuas cov pavement tshwj xeeb lossis cov khoom siv qhov chaw es tsis ua kev sib txuas txuas mus ntxiv - ntsuas qib.

 

ASTM E303-22 - British Pendulum Tester Standard

TS EN 13036-4 Kev Siv Hluav Taws Xob Hluav Taws Xob

EN 13036-4 tsev neeg kuj tseem cuam tshuam ncaj qha rau hom kev xeem no. BSI piav qhia BS EN 13036-4 raws li ib txoj hauv kev rau kev ntsuas plam / skid resistance siv lub pendulum test.

 

Qhov tseem ceeb, tus qauv piav qhia txog lub cuab yeej uas tseem nyob ruaj khov ntawm qhov chaw sim thiab ntsuas qhov chaw uas siv lub slider mounted ntawm qhov kawg ntawm ib caj npab pendulum. Nws kuj tseem sau tseg tias qhov kev ntsuas ntsuas thaj tsam me me, kwv yees li 0.01 m², thiab yog li ntawd cov txiaj ntsig yuav tsum tsis txhob muab piv nrog cov khoom siv txawb ntsuas kev sib txhuam tsis tu ncua hla ntu ntu ntev.

 

BSI - BS EN 13036-4 Pendulum Test

 

Tianpeng cov ntaub ntawv cov khoom lag luam suav nrog BS EN 1097-8, EN 13036-4: 2003, AS / NZS 4586 thiab ASTM E303 rau Pendulum Skid Tester.

 

Dab tsi yog Cov Txheej Txheem Tseem Ceeb ntawm Pendulum Skid Tester?

Ntsiab Mechanical Parameters

Cov yam ntxwv ntawm lub pendulum mechanism ncaj qha cuam tshuam rau repeatability ntawm qhov ntsuas. Tianpeng cov khoom siv cov ntaub ntawv qhia txog lub rocker / pendulum hnyav ntawm 1500 ± 30 g, qhov deb ntawm 410 ± 5 mm ntawm qhov chaw rocking center thiab qhov chaw ntawm lub ntiajteb txawj nqus, thiab ib tug 16 g roj hmab slider.

 

Cov parameter no tsis yog piav qhia tshwj xeeb xwb. Lub pendulum loj, geometry, slider yam ntxwv, thiab kev sib cuag tej yam kev mob yog ib feem ntawm cov neeg kho tshuab siv los tsim ib tug standardized ntsuas.

 

Parameter

Tianpeng specification

Vim li cas thiaj tseem ceeb

Pendulum / rocker hnyav

1500 ± 30 g

Tswj pendulum mechanical yam ntxwv

Qhov deb ntawm qhov chaw rocking center mus rau qhov chaw ntawm lub ntiajteb txawj nqus

410 ± 5 hli

Influences pendulum geometry

Roj hmab slider hnyav

16 g

Tsim cov txheej txheem tiv thaiv nto

Ntim

Aluminium alloy huab cua thauj cov ntaub ntawv

Txhawb kev thauj mus los thiab kev siv teb

Kev ntsuam xyuas

Nyob ruaj ruaj pendulum

Haum rau kev tshawb nrhiav qhov chaw hauv cheeb tsam

Nco tseg: Cov ntaub ntawv cov khoom muab rau hauv tsab xov xwm no kuj teev tus nqi siab zoo li qub. Vim hais tias chav tsev / tus nqi yuav tsum raug txheeb xyuas raws li cov ntaub ntawv tseem ceeb ua ntej tshaj tawm, nws txhob txwm tsis rov ua dua ntawm no raws li cov lus qhia meej.

 

The pendulum mass arm geometry and standardized rubber slider are fundamental components of the measurement system

Lub pendulum loj, caj npab geometry thiab cov qauv roj hmab slider yog qhov tseem ceeb ntawm kev ntsuas qhov system.

 

 

Qhov twg tuaj yeem siv Pendulum Skid Resistance Testing?

Txoj Kev thiab Pavement Surface Test

Daim ntawv thov ncaj qha tshaj plaws yog kev ntsuas pavement nto. Cov kws kho tsheb tuaj yeem siv cov cuab yeej los tshawb xyuas thaj chaw hauv cheeb tsam ntawm asphalt lossis lwm qhov chaw ntawm txoj kev uas muaj kev cuam tshuam kev sib txhuam.

 

Qhov no tuaj yeem pab tau tshwj xeeb rau kev tshuaj xyuas cov ntaub ntawv tshiab, tshawb xyuas qhov xav tias tsis tshua muaj - qhov chaw sib txhuam, sib piv cov kev kho deg sib txawv, lossis saib xyuas cov kev hloov pauv ntawm kev sib txhuam.

 

Tianpeng txheeb xyuas txoj kev kuaj saum npoo av thiab kev sim cov ntaub ntawv tshiab ntawm txoj kev hauv qab kev txhim kho ntawm cov ntawv thov ntawm nws Pendulum Skid Tester.

Kev soj ntsuam cov khoom siv kuaj

Cov cuab yeej kuj tseem siv tau rau cov qauv kuaj kom haum. Qhov no yog qhov muaj txiaj ntsig zoo thaum cov kws tshawb fawb xav sib piv qhov sib txhuam ntawm cov khoom sib txawv los yog tshawb xyuas seb qhov kev kho deg cuam tshuam li cas rau kev sib txhuam.

 

Qhov kev muaj peev xwm ntawm chav kuaj no yog qhov tseem ceeb vim tias kev ntsuas kev taug kev hauv thaj teb ib leeg tsis tuaj yeem txheeb xyuas tias vim li cas ib qho khoom ua haujlwm txawv ntawm lwm qhov.

 

Rau txoj kev dav dua -cov khoom siv kuaj, Pendulum Skid Tester tuaj yeem siv nrog Tianpeng'sAsphalt Test EquipmentthiabPob Zeb Thiab Cov Khoom Siv Sib Twtxhawm rau txuas qhov chaw- kev sib txhuam cov txiaj ntsig nrog asphalt sib tov thiab kev tshawb nrhiav aggregate.

 

Lub Pendulum Skid Tester txawv ntawm Mobile Skid li cas - Cov Khoom Siv Tiv Thaiv?

Localized Test Versus Continuous Road Surveys

Qhov kev sib txawv no tseem ceeb heev thaum xaiv cov khoom siv.

 

Lub Pendulum Skid Tester yog ib qho chaw nyob ruaj khov ntsuas ntsuas. Nws muab tso rau ntawm qhov chaw xaiv thiab ntsuas qhov kev sib txhuam ntawm qhov chaw tshwj xeeb.

 

Lub xov tooj ntawm tes skid-kev tiv thaiv, los ntawm qhov sib txawv, yog tsim los taug kev raws txoj kev taug kev thaum khaws cov kev ntsuas tsis tu ncua. Cov cuab yeej siv zoo li no yog qhov tsim nyog dua thaum lub chaw haujlwm yuav tsum tau soj ntsuam cov ntu ntev ntawm txoj kev lossis tag nrho lub network.

 

Tsis yog ob txoj kev yog universally "zoo dua." Lawv teb cov lus nug txawv engineering.

 

Kev xav tau

Pendulum Skid Tester

Mobile kev sib txhuam system

Qhov chaw kuaj

Cov ntsiab lus tshwj xeeb / cheeb tsam

Txoj kev txuas mus ntxiv

Khoom siv zog

Nyob ruaj ruaj

Tsheb -mounted/mobile

Tej daim ntawv thov

Kev tshawb nrhiav hauv zos

Kev tshawb fawb network

Laboratory siv

Yog lawm

Feem ntau txwv

Kev tshawb nrhiav hauv zos kom ntxaws

Zoo heev

Tsawg siv tau

Ntev -kev soj ntsuam pavement deb

Tsis yog npaj rau qhov no

Tsim nyog

 

EN 13036-4 cov ntaub ntawv tshwj xeeb ceeb toom tias tshwm sim los ntawm qhov chaw me me nyob ruaj ruaj pendulum sim tsis tuaj yeem tsuas yog piv nrog cov khoom siv txawb uas ntsuas skid tiv thaiv ntev li kev taug kev ntev.

 

Qhov no yog vim li cas Pendulum Skid Tester yuav tsum tau ua lag luam raws li kev soj ntsuam kev sib txhuam kev sib txhuam hauv cheeb tsam, tsis yog hloov rau lub tsheb - mounted nruam txoj kev soj ntsuam system.

 

Pendulum Skid Tester yuav tsum txhais li cas?

Tsis txhob sib piv cov kev sim sib txawv yam tsis tau kuaj xyuas cov txheej txheem

Ib qho kev ua yuam kev ntau tshaj plaws hauv kev taug kev - kev tshuaj xyuas kev sib txhuam yog kev sib piv cov lej tsim los ntawm cov tshuab ntsuas sib txawv raws li lawv zoo ib yam.

 

Ib tug British Pendulum Number yog ib tug tshwm sim nyob rau hauv ib tug txhais apparatus thiab txheej txheem. ASTM E303 qhia meej meej tias kev ntsuas los ntawm txoj kev tsis tas yuav pom zoo lossis cuam tshuam ncaj qha nrog rau lwm txoj hauv kev siv los txiav txim siab kev sib txhuam lossis kev sib tw.

 

Yog li ntawd, engineers yuav tsum xub txheeb xyuas txoj kev xeem, kev teeb tsa cov cuab yeej, slider, kuaj mob, thiab qhia chav tsev ua ntej sib piv cov txiaj ntsig.

Siv cov ntaub ntawv kev sib txhuam ua ke nrog cov xwm txheej saum npoo av

Kev ntsuas kev sib txhuam yuav muaj txiaj ntsig zoo dua thaum ua ke nrog cov ntaub ntawv hais txog kev pavement nws tus kheej. Kev sib txhuam polishing, kev sib kis ntawm qhov chaw, kev ntxhib los mos poob, dej ntws tawm, hnav, thiab lwm yam txheej txheem tuaj yeem cuam tshuam qhov kev sib txhuam.

 

Piv txwv li, yog hais tias ib tug pavement seem qhia tau hais tias tsis muaj kev sib txhuam thaum aggregate particles tshwm visibly polished, aggregate durability thiab polishing kuj yuav tsim nyog tshawb nrhiav ntxiv. Yog tias qhov kev ntxhib los mos kuj tau hloov pauv loj heev, kev kuaj kev ntxhib los mos tuaj yeem muab pov thawj ntxiv.

 

Txoj hauv kev no hloov qhov kev xeem los ntawm kev ntsuas qhov yooj yim dhau / tsis ua haujlwm rau hauv kev taug kev - cov cuab yeej kuaj mob.

 

Yuav Ua Li Cas Lub Pendulum Skid Tester Yuav Tsum Tau Saib Xyuas thiab Calibrated?

Mechanical condition ncaj qha cuam tshuam rau kev ntsuas qhov zoo

Vim tias qhov ntsuas tau nyob ntawm qhov tswj lub pendulum txav, txhua yam yuav tsum tau kuaj xyuas tsis tu ncua. Lub caj npab pendulum, slider los ua ke, tiv tauj cov khoom, kev hloov kho, thiab lub hauv paus yuav tsum nyob twj ywm hauv kev ua haujlwm zoo.

 

Cov roj hmab slider tsim nyog tau txais kev saib xyuas tshwj xeeb vim nws yog cov khoom siv ncaj qha cuam tshuam nrog qhov ntsuas qhov chaw. Nws tus mob thiab cov txheej txheem kev xeem ntawv yuav tsum tau tswj tsis tu ncua.

 

Calibration thiab pov thawj yuav tsum ua raws li tus qauv siv tau thiab cov chaw tsim khoom cov lus qhia. ASTM E303 suav nrog cov txheej txheem calibration nyob rau hauv tus qauv, txhawb ntxiv tias calibration yog ib feem ntawm txoj kev ntsuas es tsis yog ib qho kev xaiv ua haujlwm.

Vim li cas Repeatability Checks Matter

Yog hais tias rov ntsuas los ntawm tib qhov chaw npaj tau pom qhov txawv txav loj heev, tus neeg teb xov tooj yuav tsum tsis txhob cia li nruab nrab cov lej thiab txav mus. Qhov kev hloov pauv yuav qhia tau tias muaj kev teeb tsa tsis ruaj khov, qhov tsis sib xws ntawm tus swb, qhov chaw tsis sib xws, lossis lwm yam teeb meem txheej txheem.

 

Rau qhov zoo -chaw soj ntsuam tswj, khaws cov ntaub ntawv ntawm kev txheeb xyuas cov cuab yeej, ntsuas qhov xwm txheej, qhov chaw slider, qhov chaw sim, ib puag ncig thiab kev ntsuas tus kheej muab lub hauv paus muaj zog rau kev ntsuas qhov ntev - cov txiaj ntsig.

Cov ntsiab lus thiab cov lus pom zoo

Skid tsis kam ntawm txoj kev nto yuav tsum tau ntsuas nrog ib txoj kev tsim nyog rau cov lus nug engineering uas raug tshawb xyuas. Pendulum Skid Tester yog qhov tshwj xeeb tshaj yog thaum lub hom phiaj yog los ntsuas cov kev sib txhuam hauv zos ntawm qhov chaw xaiv hauv chav kuaj lossis ncaj qha rau ntawm qhov chaw.

 

Nws txoj kev khiav hauj lwm yog ncaj nraim: ib tug qauv roj hmab slider mounted ntawm lub pendulum caj npab txav mus thoob plaws qhov chaw kuaj, thiab qhov tshwm sim lub zog poob muab lub hauv paus rau kev sib txhuam ntsuas. ASTM E303 lees paub British Pendulum Tester rau kev sim thiab kev sim teb, thaum EN 13036-4 piav qhia txog txoj hauv kev nyob ruaj khov rau kev ntsuas plam / skid resistance.

 

Rau pavement engineers, tus yuam sij yog kom nkag siab qhov ntsuas qhov twg. Lub pendulum tshwm sim yuav tsum tsis txhob raug kho raws li universal kev sib txhuam coefficient los yog ncaj qha piv nrog rau kev ntsuas los ntawm mobile nruam kev sib txhuam tshuab. Hloov chaw, nws yuav tsum tau txhais nyob rau hauv cov qauv xeem uas cuam tshuam thiab txiav txim siab ua ke nrog pavement kev ntxhib los mos, cov yam ntxwv sib sau ua ke, qhov chaw saum npoo thiab lwm yam pov thawj engineering.

 

Rau cov chaw soj nstuam thiab txoj kev-cov koom haum kuaj, Tianpeng's Pendulum Skid Tester muab cov tswv yim daws teeb meem rau thaj chaw pavement thiab cov khoom siv tshuaj ntsuam kev sib txhuam, tshwj xeeb yog qhov chaw soj ntsuam kuaj thiab ntawm - yuav tsum muaj kev txheeb xyuas qhov chaw.

 

Cov lus nug nquag nug txog Pavement Skid Resistance Test

FAQ 1: Lub Pendulum Skid Tester puas tuaj yeem siv ncaj qha rau ntawm txoj kev?

Yog lawm. Pendulum Skid Tester yog tsim los ua cov cuab yeej nyob ruaj ruaj uas tuaj yeem tso rau ntawm qhov chaw xaiv pavement rau ntawm - qhov chaw sim. Nws tsis tas yuav tsum tau muab tso rau ntawm lub tsheb.

FAQ 2: Lub Pendulum Skid Tester puas tuaj yeem siv hauv chav kuaj?

Yog lawm. Txoj kev British Pendulum yog qhov tsim nyog rau kev sim thiab kev sim teb rau ntawm qhov chaw tsim nyog. ASTM E303 tshwj xeeb txheeb xyuas ob daim ntawv thov.

FAQ 3: Pendulum Skid Tester ntsuas dab tsi?

Nws ntsuas cov cuab yeej sib txhuam ntawm qhov chaw kuaj raws li lub zog poob thaum tus qauv roj hmab slider hla saum npoo. Cov txiaj ntsig tau raug nthuav tawm raws li tus lej Pendulum British raws li ASTM E303 txoj kev.

FAQ 4: Cov txiaj ntsig pendulum puas tuaj yeem sib piv ncaj qha nrog kev sib tw mobile- ntsuas ntsuas tsis kam?

Tsis yog. Ob txoj kev muaj cov qauv ntsuas sib txawv thiab cov qauv ntsuas. EN 13036-4 tshwj xeeb sau tseg tias qhov tshwm sim los ntawm nws qhov chaw me me nyob ruaj ruaj yuav tsum tsis txhob muab piv nrog cov khoom siv txawb uas ntsuas kev sib txhuam ntawm cov pav ntev ntev.

FAQ 5: Dab tsi yuav tsum tau kuaj xyuas ua ntej ua lub pendulum skid -kuaj tiv thaiv?

Tus neeg teb xov tooj yuav tsum txheeb xyuas qhov ntsuas qhov ntsuas qhov ntsuas, teeb tsa thiab kev ruaj ntseg, cov roj hmab slider thiab nws cov mob, qhov ntsuas qhov chaw, thiab qhov yuav tsum tau ua ntawm cov qauv xeem. Calibration thiab txheeb xyuas yuav tsum tau tswj raws li cov txheej txheem cuam tshuam.

Hais txog Tianpeng Test Equipment

Rau kev ua tiav pavement- kev tshawb nrhiav cov ntaub ntawv, kev ntsuas kev sib txhuam tuaj yeem ua ke nrog lwm lub tshuab kuaj kab mob:

Asphalt Test Equipment

Pob Zeb Thiab Cov Khoom Siv Sib Tw

Khoom siv kuaj

Cov khoom siv dav dav

Yog xav paub ntxiv txog cov khoom lag luam, cov kev qhia tshwj xeeb, lossis kev sib tham nrog cov kws tshaj lij ntawm peb cov cuab yeej ntsuas asphalt siab heev, thov hu rau peb pab neeg tshwj xeeb hnub no ntawmTianpeng.